MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CMT Materials REN Shape® 460 Prototype Tool & Precision Modeling Board
Categories: Polymer

Material Notes: REN Shape 460 is a moderate density precision modeling board that features a lower coefficient of thermal expansion to provide enhanced dimensional stability over a broader temperature range than other modeling boards. REN Shape 460 provides the same excellent definition and accuracy for which the REN Shape family of products is well known. Machinable with carbide cutters, REN Shape 460 features properties including:

  • Ultra-fine Surface Finish
  • Outstanding Resistance to Shrinkage and Warping
  • Superior Reproduction of Intricate Detail

Applications: REN 460 applications may include temporary or throw away master models, styling and visual models, prototypes and prototype foundry patters, vacuum form molds, architectural and automotive die models, tooling aids and fixtures, and other applications requiring fast machining and good model surfaces.

Information Provided by CMT Materials, Inc.

Key Words: Renshape
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.769 g/cc0.0278 lb/in³ASTM D-792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6464ASTM D-2240
Tensile Strength, Ultimate 12.4 MPa1800 psiASTM D-638
Flexural Strength 25.5 MPa3700 psiASTM D-790
Flexural Modulus 1.28 GPa185 ksiASTM D-790
Compressive Strength 15.2 MPa2200 psiASTM D-695
Compressive Modulus 1.25 GPa181 ksiASTM D-695
 
Thermal PropertiesMetricEnglishComments
CTE, linear 53.8 µm/m-°C
@Temperature -30.0 - 30.0 °C
29.9 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D-3386
Glass Transition Temp, Tg 104 °C219 °FASTM D-4065
 
Descriptive Properties
ColorLight Brown

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Vista Metals Duramold-5™ Cast Aluminum Mold Plate

PCMT015 / 93153

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.