MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Morgan Advanced Ceramics Unifelt™ Board 1500 Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Unifelt boards are made from refractory fiber compositions, bonded with an organic binder which begins to burn out on exposure to 180-200°C and which imparts high strength prior to heating. They show excellent flexibility properties which give good dimensional resilience after compression and make utilization of the boards or cut pieces very easy where rigid products are unsuitable. Unifelt boards are supplied in a wide range of thickness and grades each combining light weight, high heat resistance, low thermal conductivity with high sound absorption properties. Unifelt boards have excellent resistance to chemical attack, essentially unaffected by all chemicals except hydrofluoric and phosphoric acids and strong alkalis. Also after being wet by oil or water, the thermal and physical properties are fully restored on drying.

Typical Applications:

  • High temperature gaskets.
  • Brickwork linings construction joints.
  • Catalytic mufflers insulation.
  • Die cut pieces for household appliance.
  • Back up insulation for ladles.
  • Veneering modules production

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.150 g/cc
@Temperature 23.0 °C
0.00542 lb/in³
@Temperature 73.4 °F
50% RH
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.100 W/m-K
@Temperature 400 °C
0.694 BTU-in/hr-ft²-°F
@Temperature 752 °F
 0.140 W/m-K
@Temperature 600 °C
0.972 BTU-in/hr-ft²-°F
@Temperature 1110 °F
 0.200 W/m-K
@Temperature 800 °C
1.39 BTU-in/hr-ft²-°F
@Temperature 1470 °F
 0.230 W/m-K
@Temperature 1000 °C
1.60 BTU-in/hr-ft²-°F
@Temperature 1830 °F
 0.380 W/m-K
@Temperature 1200 °C
2.64 BTU-in/hr-ft²-°F
@Temperature 2190 °F
 0.500 W/m-K
@Temperature 1400 °C
3.47 BTU-in/hr-ft²-°F
@Temperature 2550 °F
Shrinkage <= 2.0 %
@Temperature 1400 °C,
Time 86400 sec
<= 2.0 %
@Temperature 2550 °F,
Time 24.0 hour
isothermal; NF-B-40-452
 
Descriptive Properties
Classification Temperature (°C)1500
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Rogers Arlon R37292S018 0.018" (0.457 mm) Cured Silicone Rubber with PTFE Coated Fiberglass Substrate
Chosun Refractories 1500 ACE BLANKET Blanket
Sinotek Materials Packing PTFE Braided with Graphite
Aremco Pyro-Putty™ 1500 High Temperature Ceramic-Metallic Putty, Ceramic Filled
Rogers Arlon CLTE Microwave Printed Circuit Board Substrate

CMORF70148 / 203446

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.