MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AGC F-Clean® Clear
Categories: Polymer; Film

Material Notes: Function:
  • F-CLEAN® Clear enables extremely high light transmission
  • It has the highest UV transmission of all greenhouse covering materials
  • It takes the full spectrum of solar light resulting in healthy crops and vivid colors
  • It has excellent light transmission at all angles of incidence
Applications:
  • For crops requiring anthocyanin such as aubergines and strawberries
  • For greenhouses growing high quality and/or high added value crops
  • For compost houses (animal manure and food leftovers)
  • For drying houses (e.g. salt, fish and plums)
  • To improve honeybee pollination

Information provided by AGC Chemicals Americas Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.75 g/ccASTM D792
Water Absorption <= 0.030 %
@Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 60.0 MPa
@Thickness 0.100 mm
JIS K7127
Elongation at Break 406 %
@Thickness 0.100 mm
JIS K7127
Tear Strength, Total 21.0 N
@Thickness 0.100 mm
Elmendorf's; JIS K7128
Tear Strength 214 kN/m
@Thickness 0.100 mm
Right Angle; JIS K7128
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+17 ohm-cmASTM D257
Dielectric Constant 2.6
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 120 kV/mmASTM D149
Dielectric Loss Index 0.00060
@Frequency 60 Hz
ASTM D150
 0.00080
@Frequency 1000 Hz
ASTM D150
 0.0050
@Frequency 1e+6 Hz
ASTM D150
 0.010
@Frequency 1.00e+18 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 94.0 µm/m-°CASTM D696
Melting Point 260 °C
Maximum Service Temperature, Air 180 °C
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 94 %
@Thickness 0.0600 mm
UV-open
UV Transmittance 89 %
@Thickness 0.0600 mm,
Wavelength 300 nm
UV-open
 
Descriptive Properties
Air Resistance120 sASTM D495

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® 305 Spectrally Transparent Epoxy
Epoxy Technology EPO-TEK® 301 Spectrally Transparent Epoxy
Tra-Con Tra-Bond F202 Spectrally Transparent High Temperature Epoxy Adhesive
Bamberger Polymers Bapolene® 4022 Polypropylene, Biaxially Oriented Film Grade
CENTROPLAST CENTROSOL Acrylonitrile butadiene Styrene copolymer

PAGCX105 / 191214

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.