MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Denka Neoprene W Polychloroprene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Neoprene Type W is a polychloroprene homopolymer, has excellent polymer stability, and a fast crystallization rate. Physical form: Chips. Color: White to Silver Gray. Distinguishing Features: General purpose - standard viscosity.

Neoprene W-type Characteristics: Raw polymers: Excellent storage stability; non-peptizable; accelerator required/cure flexibility. Vulcanizates: Good compression set resistance, good heat-aging.

General Neoprene Information: The basic chemical structure of DuPont Dow Elastomers Neoprene is polychloroprene. The polymer structure can be modified by copolymerization with sulfur or 2,3 dichloro 1,3-butadiene to yield a broad range of chemical and physical properties. All types of Neoprene resist degradation from sun, ozone, and weather; perform well in contact with oils and many chemicals; remain useful over a wide temperature range; display outstanding physical toughness, and resist burning inherently better than exclusively hydrocarbon rubbers.

Information provided by DuPont Dow Elastomers.

Denka Performance Elastomer LLC has acquired the Neoprene product line from DuPont Performance Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.23 g/cc
Viscosity Measurement 41peptized
Mooney Viscosity 40 - 49
@Temperature 100 °C
ML 1+4; ASTM D1646-81

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polychloroprene Rubber (CR)
Denka Neoprene GNA Polychloroprene
Denka Neoprene WD Polychloroprene Rubber
Denka Neoprene W-M1 Polychloroprene Rubber
Denka Neoprene WB Polychloroprene Rubber

PDVE05 / 34047

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.