LNP LUBRICOMP RFL36SXS compound is based on Nylon 6/6 resin containing 30% glass fiber, 15% PTFE. Added features of this grade include: Internally Lubricated, Wear Resistant, Heat Stabilized. Features: Internally Lubricated,Wear resistant,Heat Stabilized,Structural Information provided by SABIC |