PEARLTHANE® 12K85 LB is a standard polyester-based TPU with a lubricating additive, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mechanical properties. It is intended for extrusion related applications.All information provided by Merquinsa |