Hostacom EBS 777D WHT medium low melt flow, 1,300 MPa flexural modulus, unfilled heterophasic copolymer resin has an excellent balance of properties and processability. It is typically used for wire and cable jacketing. Applications: Wire & CableInformation provided by LyondellBasell. |