MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
PolyMirae Moplen HP521M IPP/WQBF Grade Polypropylene
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Moplen HP521M is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP521M is suitable for core resin of co-extrusion CPP film. Moplen HP521M resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for food contact.

Features: Good processability/Good optical properties/Good Stiffness

Applications: General purpose CPP/Metallizable CPP/Food and clothes packaging

Information provided by PolyMirae Company Ltd.

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
Condition L; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 100ASTM D785
Tensile Strength, Yield 360 kg(f)/cm²ASTM D638
Elongation at Yield 12 %ASTM D638
Flexural Modulus 16000 kg(f)/cm²ASTM D790
Izod Impact, Notched 3.00 kg-cm/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 110 °CASTM D648
Vicat Softening Point 155 °CASTM D1525
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem H 504 XP Bioriented Film Polypropylene
Hyosung Topilene F600 PP
Braskem H 401 Cast Film Extrusion Polypropylene
LyondellBasell Moplen HP528N Polypropylene
Formosa Plastics Formolene® 4101M Staple Fiber and Injection Molding Polypropylene

PMIRAE35 / 53147

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.