MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Pyrotek I-14 Insulating Board
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Pyrotek's I-14 is a low density hydrous calcium silicate board which features exceptional strength and low thermal conductivity. Inorganic and incombustible, I-14 also contains no RDF's.

Applications

  • Thermal insulation
  • Pot bake out panels
  • Backup insulation

Advantages

  • Exceptional strength
  • Asbestos-free
  • Easily cut to specifications
  • Composed of incombustible, inorganic material

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.256 g/cc0.00925 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 0.700 MPa102 psi
Compressive Strength 0.700 MPa102 psiat 5% deformation
 0.900 MPa131 psiat 10% deformation
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.0600 W/m-K
@Temperature 93.0 °C
0.416 BTU-in/hr-ft²-°F
@Temperature 199 °F
 0.0700 W/m-K
@Temperature 204 °C
0.486 BTU-in/hr-ft²-°F
@Temperature 399 °F
 0.100 W/m-K
@Temperature 316 °C
0.694 BTU-in/hr-ft²-°F
@Temperature 601 °F
 0.130 W/m-K
@Temperature 427 °C
0.902 BTU-in/hr-ft²-°F
@Temperature 801 °F
Maximum Service Temperature, Air 927 °C1700 °FContinuous

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CPYRO161 / 1879

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.