MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polynt 24 CFP40-400g Carbon Fiber VE Fleece
Categories: Polymer; Thermoset; Vinyl Ester

Material Notes: Recycled molding compound based on vinyl ester resin and reinforced with pyrolized carbon fleece designed for compression molding technology. These material with a weight reduced potential and a high design freedom enter different areas for structural application where high mechanical properties are requested.

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.36 g/ccISO 1183 A
Filler Content 40 %Carbon Fleece
Linear Mold Shrinkage 0.00050 cm/cmISO 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 195 MPaISO 527-4
Tensile Modulus 26000 MPaISO 527-4
Flexural Strength 260 MPaISO 14125
Flexural Modulus 24300 MPaISO 14125
Tensile Impact Strength 15.0 kJ/m²ISO 179
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) >= 200 °CISO 75-2
Glass Transition Temp, Tg 170 °CISO 11357-2
 
Processing PropertiesOriginal ValueComments
Hold Pressure 1160 - 1740 psiMolding pressure
Cure Time 35.0 sec
@Temperature 125 - 140 °C
per mm
Shelf Life 2.00 Month
@Temperature 23.0 °C
 6.00 Month
@Temperature -18.0 °C
 
Descriptive Properties
Fiber length25 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPOLYN9085 / 231680

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.