MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ineos N05U-00 Polypropylene Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer; Polypropylene, Impact Modified; Molded/Extruded

Material Notes: This is an extrusion-grade nucleated impact copolymer polypropylene resin designed for fiber optic buffer tube applications in the protection of glass fibers. It also has an excellent impact/stiffness property balance and provides the high compression strength required to meet the Bellcore GR-20-CORE standard (Generic Requirements for Optical Fiber and Fiber Optic Cable).

    Applications
  • Buffer tubes
  • Filler rods
  • Core jackets

    Benefits
  • Oxidative stability
  • UV stabilized
  • ESCR
  • Good balance of stiffness and impact strength

Information provided by Ineos Olefins & Polymers USA

Key Words: Excellent impact/stiffness property balance
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.909 g/ccASTM D792
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 89ASTM D785
Tensile Strength at Break 2790 psi2.0 in/min; ASTM D638
Tensile Strength, Yield 3900 psi2.0 in/min; ASTM D638
Elongation at Break 130 %2.0 in/min; ASTM D638
Elongation at Yield 5.2 %2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 216000 psiASTM D790A
Izod Impact, Notched 1.20 ft-lb/in
@Temperature -20.0 °C
ASTM D256
 7.40 ft-lb/in
@Temperature 22.8 °C
ASTM D256
Izod Impact, Notched (ISO) 2.95 ft-lb/in²
@Temperature -20.0 °C
Area; ASTM D256
 18.4 ft-lb/in²
@Temperature 22.8 °C
Area; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 223 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 135 °FUnannealed; ASTM D648
Vicat Softening Point 304 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Gloss 64 %60°; ASTM D2457
 
Descriptive Properties
ProcessExtrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ineos R01C-01 Polypropylene Random Copolymer
Ineos N02G-00 Polypropylene Impact Copolymer
Ineos N05G-00 Polypropylene Impact Copolymer
Ineos N00M-00 Polypropylene Impact Copolymer
Ineos L12Z-01 Polypropylene Impact Copolymer

PINEOS057 / 99378

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.