MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Eastman EB Acetate
Categories: Other Engineering Material

Material Notes: CAS No. 112-07-2

Product Description: Eastman™ EB Acetate (Ethylene Glycol Monobutyl Ether Acetate) is a high boiling glycol etherester. Its slow evaporation rate provides excellent flow and leveling in high-bake coatings as well as air-dry systems such as epoxy coatings. It has limited water miscibility. It is supplied as a urethane grade solvent. The chemical substances for this product are listed as Inert Ingredients Permitted for Use in Nonfood Use Pesticide Products under the Federal Insecticide, Fungicide, and Rodenticide Act (FIFRA).

Application/Uses:

  • Coatings - Architectural
  • Coatings - Automotive OEM
  • Coatings - Automotive Refinish
  • Coatings - Can and Coil
  • Coatings - Consumer Electronics
  • Coatings - General Industrial
  • Coatings - Industrial Maintenance and Marine
  • Coatings - Industrial Wood
  • Coatings - Transportation
  • Graphic Arts - Printing Inks
Key Attributes:
  • Efficient coalescent
  • Excellent solvent activity
  • High blush resistance
  • High electrical resistance
  • Inert - Nonfood use
  • Readily biodegradable
  • Slow evaporation rate
  • Urethane grade

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.941 g/cc
Viscosity 1.8 cPLiquid
Molecular Weight 160.21 g/mol
Vapor Pressure 0.000382 atm
@Temperature 20.0 °C
 0.00759 atm
@Temperature 55.0 °C
Surface Tension 30.3 dynes/cm
 
Chemical PropertiesOriginal ValueComments
Critical Pressure 24.5 atm
Critical Temperature 361.7 °C
Total Acid Number <= 0.010
 
Thermal PropertiesOriginal ValueComments
CTE, linear 104 µm/m-°C
Melting Point -64.0 °CFreezing Point
Boiling Point 186 °C@ 760 mm Hg, Initial
 194 °C@ 760 mm Hg, Dry Point
Flash Point 71.0 °CTag Closed Cup
 81.0 °CTag Open Cup
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.4142
 
Descriptive Properties
ColorPt-Co

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM5223 / 222417

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.