MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polynt BathCote® 992 Base, White Sanitary Gel Coat
Categories: Polymer; Thermoset

Material Notes: BathCote® 992 gel coats are high performance products formulated for the sanitary-ware industries. These gel coats have low volatile organic compound properties. BathCote® gel coats meet the EPA National Emission Standards for Hazardous Air Pollutants (NESHAP): Reinforced Composites Construction. While offering these benefits, Polynt Composites gel coats have retained the important construction application qualities customers have come to expect from Polynt Composites gel coats, such as resistance to porosity, tearing, and color separation; sag resistance; consistent liquid properties; good patchability; and more. These all add up to higher quality appeal in FRP parts made from Polynt Composites' 992 Series gel coats. The BathCote® 992 series resist blistering because they are formulated to provide high performance against water and certain chemicals. These gel coats were primarily developed for sanitary applications. These gel coats provide durable, reduced maintenance products. Polynt Composites gel coats have enabled customers to meet and surpass all requirements of the American National Standard for plastic bathtubs, shower receptors and shower stalls, IAPMO/ANSI Z124.1 .2 -2005, Section 6.1. This product series has received certification from the Canadian Standards Association (CSA) and is eligible to bear the CSA trademark. These gel coats require only the addition of the proper amount of the appropriate methyl ethyl ketone peroxide to cure.

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Brookfield Viscosity 3200 - 3500 cP3200 - 3500 cPRVF #4 spindle @ 20 rpm
 
Thermal PropertiesMetricEnglishComments
Flash Point 31.1 °C88.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 30.0 - 45.0 min0.500 - 0.750 hourLay-up Time
Gel Time 3.50 - 10.0 min
@Temperature 25.0 °C
3.50 - 10.0 min
@Temperature 77.0 °F
Method POLYNT-22-TAS-TM-515.2, 100 g mass, 77°F with United Initiators Norox® 1.8% MEKP
 
Descriptive Properties
Sag ResistanceGood at 20 mils
Thixotropic Index4.5-5.52/20 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLYN9191 / 231786

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.