MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Borealis Queo™ 0201 Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Queo 0201 is an ethylene based octene-1 plastomer, produced in a solution polymerization process using a metallocene catalyst. CAS-No. 26221-73-8

Special Features: Queo 0201 is optimized to deliver:

  • Excellent environmental stress cracking resistance (ESCR)
  • High clarity
  • Flexibility
  • Versatile blending with other polyolefins in film, extrusion and molding applications.
  • Unrivalled sealing and hot tack properties at low temperature
  • Low amount of extractables
  • Outstanding toughness
  • Outstanding puncture resistance
  • Low temperature impact strength
Applications:
  • Seal layers in lamination and flexible barrier films
  • High strength flexible films
  • Heat shrinkable display film
  • Specialty stretch film applications
  • PP film toughness modification
  • Roof coverings
  • Tunnel linings
  • Flexible low voltage insulation
  • Halogen free flame retardant compounds
  • Blow molding
  • Soft foams, e.g. artificial wine corks
Additives: Queo 0201 contains processing stabilizers

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.902 g/cc0.0326 lb/in³ISO 1183
Viscosity  300 cP
@Shear Rate 1000 1/s,
Temperature 230 °C
300 cP
@Shear Rate 1000 1/s,
Temperature 446 °F
DIN 54811
 400 cP
@Shear Rate 1000 1/s,
Temperature 190 °C
400 cP
@Shear Rate 1000 1/s,
Temperature 374 °F
DIN 54811
 1000 cP
@Shear Rate 100 1/s,
Temperature 230 °C
1000 cP
@Shear Rate 100 1/s,
Temperature 446 °F
DIN 54811
 3000 cP
@Shear Rate 10.0 1/s,
Temperature 190 °C
3000 cP
@Shear Rate 10.0 1/s,
Temperature 374 °F
DIN 54811
Environmental Stress Crack Resistance >= 1000 hour>= 1000 hourASTM D 1693-B
Melt Flow 1.10 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.10 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 43.043.0ISO 868
Tensile Strength 36.0 MPa5220 psiISO 527-2
Elongation at Break 715 %715 %ISO 527-2
Tensile Modulus 0.0650 GPa9.43 ksiASTM D 882-A
Flexural Modulus 0.0720 GPa10.4 ksiISO 178
Izod Impact, Notched (ISO) NBNBISO 180/1A
Dart Drop Total Energy 2800 J/cm5.25 ft-lb/mil[mJ/mm], Energy to break
Dart Drop >= 48.0 g/micron>= 1220 g/milASTM D1709
Heat Seal Strength Initiation Temperature 78.0 °C172 °FASTM F88
 
Thermal PropertiesMetricEnglishComments
Melting Point 97.0 °C207 °FISO 11357-3
Vicat Softening Point 82.0 °C
@Load 1.02 kg
180 °F
@Load 2.25 lb
ISO 306
Brittleness Temperature <= -90.0 °C<= -130 °FASTM D 746
 
Optical PropertiesMetricEnglishComments
Haze 2.00 %2.00 %ASTM D1003
Gloss 84.0 %84.0 %45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBORE9883 / 323240

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.