Purell PE GF4760 is a high density polyethylene with good ESCR, high rigidity and good organoleptic properties. It contains antioxidants and is delivered in pellet form. The grade is used for small blow moldings for foodstuff, consumer goods as well as pharmaceutical packaging. This grade is also well established for injection blow molding applications. Applications: Bottles and Vials, Diagnostic Applications, Healthcare Applications, Medical DevicesInformation provided by LyondellBasell. |