MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
American Red Western Cedar (Giant Arborvitae) Wood
Categories: Wood and Natural Products; Wood; Softwood

Material Notes: An acidic timber which may corrode metals under damp conditions and cause iron staining. Conifer
Usual surface texture: Coarse
Dimensional changes when dried lumber is subjected to variations in humidity during service: Small
Resistance to fungal decay (Heartwood in ground contact): Durable (15 to 25 years)
Resistance to penetration by preservatives: Resistant
Common Applications: Shingles, exterior cladding, greenhouses, beehives

Property values marked by an asterisk (*) have been taken from an unusually old reference source.

Key Words: Thuja plicata; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.310 g/ccOven Dry Weight/Unseasoned Volume
 0.330 g/ccAir Dry (12-15% Moisture Content)
 27.0 lb/ft³Unseasoned*
Moisture Absorption at Equilibrium 1.5 - 8.0 %Between 40% RH and 90% RH
Cell Length 7.00 mmMature Wood
 
Mechanical PropertiesOriginal ValueComments
Hardness, Wood Indentation 1200 NSide. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 1600 NSide
 1900 NEnd. Force required to imbed a 0.444 inch steel ball to one-half its diameter
Tensile Strength, Ultimate 1.50 MPaPerpendicular to Grain
Modulus of Rupture 0.0530 GPaStatic Bending
 5.20 ksiStatic Bending*
Flexural Yield Strength 3300 psiFiber Stress at Elastic Limit; Static Bending*
Flexural Modulus 7.73 GPaStatic Bending
 950 ksiStatic Bending*
Compressive Strength 4.20 MPaPerpendicular to Grain
 43.0 MPaParallel to Grain
 310 psiPerpendicular to Grain*
 2500 psiParallel to Grain*
 2840 psiMax Crushing Strength Parallel to Grain*
Poissons Ratio 0.296µLT, 12% Moisture Content
 0.378µLR, 12% Moisture Content
 0.403µTR, 12% Moisture Content
 0.484µRT, 12% Moisture Content
Machinability 100 %Good Relative to Other Wood
Shear Strength 5.90 MPaOrientation Unknown
 720 psiParallel to Grain*
Impact 2.4in-lb/in³; Work to Elastic Limit; Unseasoned Sample; Impact Bending*
 7100psi; Fiber Stress at Elastic Limit; Unseasoned Sample; Impact Bending*
Work to Elastic Limit 0.640 in-lb/in³Static Bending*
Work to Maximum Load 5.00 in-lb/in³Static Bending*
Toughness 10.2 JRadial
 14.7 JTangential
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.570 BTU-in/hr-ft²-°FOven Dry
 0.680 BTU-in/hr-ft²-°F12% Moisture Content
Shrinkage 2.4 %Radial; Green to Zero Moisture
 2.4 %Tangential; Unseasoned to Oven Dry*
 4.4 %Tangential; Green to Zero Moisture
 6.8 %Volumetric; Green to Zero Moisture
 7.6 %Radial; Unseasoned to Oven Dry*
 23 %Volumetric; Unseasoned to Oven Dry*
 
Descriptive Properties
ColorReddish brownUsual for heartwood

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
American Red Spruce Wood
Red Pine Wood
American Northern White Cedar (Eastern Arborvitae) Wood
American Sitka Spruce Wood
American Balsam Fir Wood

PTSA550 / 71262

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.