MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
A. Schulman BMC 2270 Mineral Filled, Glass Reinforced Polyester
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass and Mineral Filled BMC

Material Notes: BMC 2270 molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression and transfer molding. It is a general purpose material with medium impact strength and wet insulation resistance.

Typical applications include distributor caps and rotors.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.86 g/cc
Water Absorption 0.12 %24 hours, 23°C
Linear Mold Shrinkage 0.0025 - 0.0035 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 25 - 35
Tensile Strength, Ultimate 5000 - 7000 psi
Flexural Strength 15000 - 20000 psi
Compressive Strength 22000 - 25000 psi
Izod Impact, Notched 3.00 - 4.00 ft-lb/in
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 5.3
@Frequency 60 Hz
Dielectric Strength 375 V/milShort Time
Dissipation Factor 0.018
@Frequency 60 Hz
Arc Resistance 190 sec
Comparative Tracking Index >= 500 V
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) >= 500 °F
Flammability, UL94 V-0
@Thickness 6.35 mm
 V-0
@Thickness 3.17 mm
 V-0
@Thickness 1.59 mm
 
Processing PropertiesOriginal ValueComments
Mold Temperature 280 - 330 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
G-10 Fiberglass Epoxy Laminate Sheet
A. Schulman BMC 685 Mineral Filled, Glass Fiber Reinforced Polyester Compound
A. Schulman BMC 695 Vinyl Ester Molding Compound
A. Schulman BMC SLC 1000 Glass Reinforced Polyester
A. Schulman BMC A50-XHS High Strength Grade Molding Compound

PBMC059 / 27242

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.