BMC T60-6006 is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost per cubic inch savings. BMC T60-6006 can be injection, transfer and compression molded. It is UL listed and is typically used in power distribution equipment, switching components/relays, constant use switch applications and circuit protection breakers. Information provided by Bulk Molding Compounds, Inc. |