MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Arkema Lacovyl® GA 9028 Vinyl Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); Polyvinyl Chloride - Polyvinyl Acetate Copolymer

Material Notes: LACOVYL GA 9028 is a copolymer of vinyl chloride and vinyl acetate produced by suspension polymerization process. It may be used by itself or blended with a PVC homopolymer of similar molecular weight.

Its characteristics are :

  • Vinyl acetate content:10.5%. Viscosity index (ISO 1628-2):85 ml/g,(K value:59). Apparent density (ISO 60):0.59 g/ml.
  • ease of fusion.
  • good elongation with heat.
  • high level of fluidity in the molten state.

Facilitating the extrusion or calendering of films or rigid sheets and improving their suitability for thermoforming. It is furthermore perfectly compatible with the additives used to improve impact resistance. LACOVYL GA 9028 has a very good base color and excellent thermal stability with the stabilizers currently used, especially with those suitable for the manufacture of food containers.

* RECOMMENDED APPLICATIONS

  • Calendering or extrusion of rigid sheets and films for:
  • packaging or display packs made by thermoforming
  • boxes
  • stationary - credit cards, playing cards - computer disc and video-cassettes holders
  • sleeves for bottles
  • Records molding (addition resin).

ISO data provided by the manufacturer, Arkema.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Apparent Bulk Density 0.590 g/cc
Viscosity Number 85 cm³/g

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema Lacovyl® GA 7701 Vinyl Copolymer
Arkema Lacovyl® GA 7701 H Vinyl Copolymer
Arkema Lacovyl® PA 1384 Vinyl Copolymer
Arkema Lacovyl® EF 821 PVC
Arkema Lacovyl® EF 701 PVC

PZARKG274 / 25568

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.