MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Arkema Kynar Flex® 3030-10 PVDF
Material Notes:

Information provided by Arkema.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.78 - 1.82 g/cc1.78 - 1.82 g/ccASTM D792
Water Absorption <= 0.050 %<= 0.050 %ASTM D570
Viscosity 700000 - 1.30e+6 cP
@Shear Rate 100 1/s,
Temperature 230 °C
700000 - 1.30e+6 cP
@Shear Rate 100 1/s,
Temperature 446 °F
Melt; ASTM D3835
Melt Flow 8.0 - 25 g/10 min
@Load 3.80 kg,
Temperature 230 °C
8.0 - 25 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 45 - 5545 - 55ASTM D2240
Tensile Strength at Break 19.3 - 24.8 MPa2800 - 3600 psiASTM D638
Tensile Strength, Yield 12.0 MPa1740 psiDry; ISO 527-1/-2
 12.4 - 16.5 MPa1800 - 2390 psiASTM D638
Elongation at Break >= 50 %>= 50 %Dry; ISO 527-1/-2
 <= 500 %<= 500 %ASTM D638
Elongation at Yield 30 %30 %Dry; ISO 527-1/-2
 25 - 40 %25 - 40 %ASTM D638
Tensile Modulus 0.207 - 0.345 GPa30.0 - 50.0 ksiASTM D638
 0.283 GPa41.0 ksiDry; ISO 527-1/-2
Flexural Modulus 0.241 - 0.379 GPa35.0 - 55.0 ksiASTM D790
Izod Impact, Notched NBNBASTM D256
Charpy Impact, Notched NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Dry; ISO 179/1eA
Taber Abrasion, mg/1000 Cycles 28 - 3328 - 33CS 17 1000g:pad; ASTM-G195-13A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+14 ohm-cm2.00e+14 ohm-cmDry; IEC 60093
Surface Resistivity per Square 7.60e+11 - 7.80e+11 ohm7.60e+11 - 7.80e+11 ohmASTM D257
Dielectric Strength 1.00 - 1.20 kV/mm25.4 - 30.5 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 153 - 194 µm/m-°C85.0 - 108 µin/in-°FASTM D696
Melting Point 160 - 168 °C320 - 334 °FASTM D3418
 164 °C327 °F10°C/min; Dry; ISO 11357-1/-3
Glass Transition Temp, Tg -42.0 °C-43.6 °F10°C/min; Dry; ISO 11357-1/-2
 -40.0 °C-40.0 °FASTM D7028
Flammability, UL94 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
IEC 60695-11-10
Oxygen Index 42 %42 %ASTM D2863
 45 %45 %Dry; ISO 4589-1/-2
 
Descriptive Properties
Moisture SensitiveNo

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Kynar Flex® 2850 WR PVDF
Arkema Kynar Flex® PPA 2200 PVDF
Arkema Kynar® 705 PVDF
Arkema Kynar Flex® 3030-15 PVDF
Arkema Kynar Flex® Ultraflex B PVDF

PARKF713 / 193517

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.