MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Idemitsu Kosan Xarec® WA 214 SPS, 40% Glass Filled  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Syndiotactic Polystyrene (SPS); Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.37 g/cc
Filler Content 40 %
Moisture Absorption 0.010 %24 hrs., 50% RH
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
Linear Mold Shrinkage, Transverse 0.0020 - 0.0040 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 145 MPa
Elongation at Break 1.5 %
Tensile Modulus 13.7 GPa
Flexural Yield Strength 220 MPa
Flexural Modulus 13.2 GPa
Izod Impact, Notched (ISO) 11.0 kJ/m²
Izod Impact, Unnotched (ISO) 40.0 kJ/m²
Charpy Impact Unnotched 42.0 kJ/m²
Charpy Impact, Notched 12.0 kJ/m²
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+16 ohm-cm
Dielectric Constant 3.1
Dielectric Strength 26.0 kV/mmASTM D145
Dissipation Factor 0.0010IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 15.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
CTE, linear, Transverse to Flow 38.0 µm/m-°C
Deflection Temperature at 0.46 MPa (66 psi) 270 °C
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
Flammability, UL94 HB
@Thickness 0.750 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 - 310 °C
Mold Temperature 50.0 - 80.0 °C
 130 - 155 °CFor optimal surface finish

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Idemitsu Kosan Xarec® WA 214LG SPS, 40% Glass Filled
Idemitsu Kosan Xarec® EA 543 SPS, 40% Glass Filled
Idemitsu Kosan Xarec® WA 204 SPS, 20% Glass Filled
Idemitsu Kosan Xarec® N WA 7030 SPS, 30% Glass Filled
Idemitsu Kosan Xarec® N WA 5030 SPS, 30% Glass Filled

PIDEM110z / 171615

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.