MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese SO.F.TER Sofprene® Z PCV Free Boots 23 Z For Upper
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: Boots

Information provided by SO.F.TER. Spa

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.990 g/ccASTM D 792
Linear Mold Shrinkage 0.0010 cm/cm
Melt Flow 150 g/10 minASTM 1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 40ASTM D 2240
Elongation at Break 480 %ASTM D412
 
Processing PropertiesOriginal ValueComments
Processing Temperature 160 - 180 °C
 
Descriptive Properties
CharacteristicsBoots, for upper, covered
Featuresavailable in all colors, can be sewed and milled
Surface Appearancesemi matte

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for PVC, Rigid Grade
Overview of materials for PVC, Molded
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
Colorite Polymers 5011G-015 (Extrustion), 5012G-015 (Molding) Radiation Sterilizable Vinyl Compound
Colorite Polymers 4011G-015 (Extrustion), 4012G-015 (Molding) Radiation Sterilizable Vinyl Compound

PSOFS640 / 162104

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.