MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
BASF 3D Ultrafuse® PET CF15 Fused Fillament, 15% Carbon Fiber Reinforced
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Components: Acrylonitrile Polyethylene Terephthalate based filament filled with 15% carbon fiber for Fused Filament Fabrication.

Product Description: PET CF15 is a Carbon Fiber reinforced PET which has precisely tuned material properties, for a wide range of technical applications. The filament is very strong and stiff and has high heat resistance. With its high dimensional stability and low abrasiveness, the filament offers an easy to print experience which allows direct printing on glass or a PEI sheet. It is compatible with HiPS for breakaway support and water soluble support and has an excellent surface finish.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.366 g/ccPrinted Part; ISO 1183-1
Melt Flow 34.15 g/10 min
@Load 2.16 kg,
Temperature 260 °C
ISO 1133
Storage Temperature 15.0 - 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 12.5 MPaZX: Upright; ISO 527
 63.2 MPaXY: Flat; ISO 527
Elongation at Break 0.50 %ZX: Upright; ISO 527
 3.7 %XY: Flat; ISO 527
Modulus of Elasticity 2.822 GPaYoung's, ZX: Upright; ISO 527
 6.178 GPaYoung's, XY: Flat; ISO 527
Flexural Strength 19.7 MPaZX: Upright; ISO 178
 108 MPaXY: Flat; ISO 178
 145 MPaXZ: On its edge; ISO 178
Flexural Modulus 2253 MPaZX: Upright; ISO 178
 5452 MPaXY: Flat; ISO 178
 6293 MPaXZ: On its edge; ISO 178
Flexural Strain at Break 0.90 %ZX: Upright; ISO 178
 2.8 %XZ: On its edge; ISO 178
 3.7 %XY: Flat; ISO 178
Izod Impact, Notched (ISO) 2.00 kJ/m²ZX: Upright; ISO 180
 5.00 kJ/m²XZ: On its edge; ISO 180
 5.70 kJ/m²XY: Flat; ISO 180
Izod Impact, Unnotched (ISO) 2.40 kJ/m²ZX: Upright; ISO 180
 22.6 kJ/m²XZ: On its edge; ISO 180
 25.1 kJ/m²XY: Flat; ISO 180
Charpy Impact Unnotched 1.30 kJ/m²ZX: Upright; ISO 179-2
 27.8 kJ/m²XY: Flat; ISO 179-2
 32.0 kJ/m²XZ: On its edge; ISO 179-2
Charpy Impact, Notched 0.500 kJ/m²ZX: Upright; ISO 179-2
 4.80 kJ/m²XZ: On its edge; ISO 179-2
 5.40 kJ/m²XY: Flat; ISO 179-2
 
Thermal PropertiesOriginal ValueComments
Melting Point 245 °CISO 11357-3
Crystallization Temperature 204 °CISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 108 °CISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °CISO 75-2
Glass Transition Temp, Tg 79.0 °CISO 11357-2
 
Processing PropertiesOriginal ValueComments
Processing Temperature 65.0 - 85.0 °CBed, Bed Material: Glass, PEI
Nozzle Temperature 250 - 270 °C
Drying Temperature 65.0 °Cin a hot air dryer or vacuum oven
Dry Time 4.00 - 16.0 hour
Shelf Life 12.0 Month
 
Descriptive Properties
Nozzle Diameter=0.6 mm
Print speed30-60 mm/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBASF3D008 / 312249

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.