MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
General Plastics LAST-A-FOAM® TR-24 Polyurethane Foam
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes:

Information provided by General Plastics Manufacturing Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.384 g/ccASTM D1623
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 47.6ASTM D2240
Tensile Strength 921 psiPerpendicular to Rise; ASTM D1623
 1036 psiParallel to Rise; ASTM D1623
Tensile Modulus 108902 psiParallel to Rise; ASTM D1623
 134462 psiPerpendicular to Rise; ASTM D1623
Flexural Strength 1316 psiRise Parallel to Test Span; ASTM D790
 1334 psiRise Parallel to Beam Thick.; ASTM D790
Flexural Modulus 45871 psiRise Parallel to Beam Thick.; ASTM D790
 52195 psiRise Parallel to Test Span; ASTM D790
Compressive Strength 1090 psi
@Temperature 71.1 °C
Perpendicular to Rise; ASTM D1621
 1130 psi
@Temperature 71.1 °C
Parallel to Rise; ASTM D1621
 1479 psi
@Temperature 23.9 °C
Parallel to Rise; ASTM D1621
 1484 psi
@Temperature 23.9 °C
Perpendicular to Rise; ASTM D1621
 2364 psi
@Temperature -51.1 °C
Perpendicular to Rise; ASTM D1621
 2368 psi
@Temperature -51.1 °C
Parallel to Rise; ASTM D1621
Compressive Modulus 34609 psi
@Temperature 71.1 °C
Parallel to Rise; ASTM D1621
 34654 psi
@Temperature 71.1 °C
Perpendicular to Rise; ASTM D1621
 41228 psi
@Temperature 23.9 °C
Perpendicular to Rise; ASTM D1621
 47028 psi
@Temperature -51.1 °C
Parallel to Rise; ASTM D1621
 48725 psi
@Temperature 23.9 °C
Parallel to Rise; ASTM D1621
 50052 psi
@Temperature -51.1 °C
Perpendicular to Rise; ASTM D1621
Poissons Ratio 0.30
Shear Modulus 12.162 ksiRise Parallel to Specimen Length; ASTM C273
 13.542 ksiRise Parallel to Specimen Thickness; ASTM C273
Shear Strength 0.885 ksiRise Parallel to Specimen Length; ASTM C273
 0.890 ksiRise Parallel to Specimen Thickness; ASTM C273
 
Thermal PropertiesOriginal ValueComments
CTE, linear 32.0 µin/in-°F
@Temperature -28.9 - 71.1 °C
GP Method
Thermal Conductivity 0.453 BTU-in/hr-ft²-°FASTM C518
Glass Transition Temp, Tg 256 °FASTM E1824
 
Descriptive Properties
Closed Cell Content97.5%ASTM D2856 Procedure B
Tumbling Friability (%)0.920 mins at 60 rpm, ASTM C421

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M RPF-C (0.32 g/cc) (Reinforced Polyurethane Foam) Continuous Strand Fiberglass
3M RPF-C (0.24 g/cc) (Reinforced Polyurethane Foam) Continuous Strand Fiberglass
General Plastics LAST-A-FOAM® R-9320 Thermal Isolation Blocks
General Plastics LAST-A-FOAM® TR-20 Polyurethane Foam
ITW Insulation TRYMER® 200L Polyisocyanurate Foam

PGENR071 / 186857

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.