BK1005 only as of June 2000.- Features: Antistatic, ECO Compliant
- Forms: Pellets
- Processing Method: Injection Molding
Information provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names instituted after the SABIC purchase. |