MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
C.O.I.M. FILCO® 350 Non Ionic Unsaturated Polyester Polymer Emulsion for Glass Fiber Sizing
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic

Material Notes: Non Ionic Unsaturated Polyester Polymer Aqueous Emulsion for Glass Fiber Sizing
General Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and are collectively known as FILCO®. The products in the FILCO® line serve to size glass fiber, to optimize the mechanical characteristics of the fiber, or to bind the fibers for the production of mat.
Applications: Filco 350 has been studied as a primary film forming component of glass fiber sizing for unsaturated polyester matrix strengthening.
Consider the following special properties:
  • pseudo-glass consistency of film
  • good solubility in vinylic solvents
  • good compatibility with other typical sizing component formulations
  • good compatibility with various unsaturated polyester matrixes
  • good transparency of reinforced compounds
  • high impregnation speed of sized fibers during glass/resin compound preparation

It is recommendable to use Filco 350 in combination with metacrylic radical organosilanes for glass fiber sizing formulation for:
  • roving for translucent sheets
  • roving for chip/spray
  • chopped strand mat with powder and liquid binder highly soluble in styrene

Information provided by P.A.T. Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 44 - 46 %
pH 2.0 - 4.0
Brookfield Viscosity 50 - 250 cP
@Temperature 20.0 °C
Brookfield RVT spindle 2.2 RPM
 
Descriptive Properties
AppearanceMilky Liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
C.O.I.M. FILCO® 362 Film Former for Glass Fiber Sizes
C.O.I.M. FILCO® 300 Non Ionic Epoxy-Polyester Aqueous Emulsion for Glass Fiber Sizing
C.O.I.M. FILCO® 339 Film Former for Glass Fiber Sizes
C.O.I.M. FILCO® 306 Film Former for Glass Fiber Sizes
C.O.I.M. FILCO® 309 Film Former for Glass Fiber Sizes

PCOIM105 / 28708

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.