MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Imerys Minspar™ 3 Ground Feldspar
Categories: Ceramic; Clay; Feldspar Clay

Material Notes: Minspar™ 3 is a coarse particle size, ground Feldspar with a tightly controlled particle size distribution. The angular particle shape and inherent cheMical resistance make Minspar™ 3 an excellent mineral additive for adhesives and sealants and for flattening efficiency in interior and exterior finishes and primers.

Information provided by Imerys

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.60 g/cc
Bulk Density 45.0 lb/ft³loose
 70.0 lb/ft³packed
Density 21.6 lb/galsolid
Brightness 89.5 %G.E. Brightness
Particle Size 12 µmmean
Particle Mesh Size 325 Mesh4% retained
pH 8.710% solids
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 6.0
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.53
 
Component Elements PropertiesOriginal ValueComments
H2O, Water 0.10 %
 
Descriptive Properties
Hegman Grind1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Imerys Minspar™ 10 Ground Feldspar
Imerys Minspar™ 7 Ground Feldspar
Imerys Minspar™ 4 Ground Feldspar
World Minerals Celite® Super Fine® Super Floss Diatomaceous Earth Antiblock Additive
PPT BP2000 NiZn Ferrite Powder

CIMERY009 / 88359

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.