LNP FARADEX WX08014 compound is based on Polybutylene Terephthalate (PBT) resin containing stainless steel fiber. Added features of this grade include: EMI/RFI shielding, Electrically Conductive, Flame Retardant. Features: EMI/RFI Shielding,Flame Retardant,Electrically Conductive Information provided by SABIC |