MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Rogers Arlon 440-638RF 0.0055" (0.140 mm) Style 1165 Plain Weave, Prime Coated Fiberglass
Categories: Ceramic; Glass; Glass Fiber

Material Notes: Design/Construction:
Fiberglass Fabric primed for adhesion to silicone elastomers vulcanized with organic peroxides.
Material: Prime Coated Fiberglass

Count: 60x52 (Ends x Picks)

This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 5.50 milOverall; Arlon SQA-TMS-003
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 450 °F
Minimum Service Temperature, Air -70.0 °F
 
Processing PropertiesOriginal ValueComments
Shelf Life 60.0 Month
@Temperature 23.9 °C
From date of manufacture
 
Descriptive Properties
ColorRed
Total Product Weight (oz/yd2)3.9Arlon SQA-TMS-025
Uncoated Fabric Break Strength100 lb/inArlon SQA-TMS-026, Warp Direction, Substrate Property
 140 lb/inArlon SQA-TMS-026, Fill Direction, Substrate Property

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DIAB Divinycell® P 100 Sandwich Core Material
E-Glass Fiber, Generic
3A Composites Core Materials AIREX® T90.100 Easy Processing Structural FST Foam
3A Composites Core Materials AIREX® R82.80 High Performance Structural Foam
COI Ceramics Nextel™ AS-N312 Oxide Ceramic Matrix Composite, Aluminosilicate

PARL188 / 125374

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.