MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics Superwool® HT Unifelt™ Board Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Superwool ® HT Unifelt™ boards are made of Superwool ® HT fibers compositions, bonded with an organic binder which begins to burn out on exposure to 180-200°C (356-392°F) and which imparts high strength prior to heating. They show excellent flexibility properties which give good dimensional resilience after compression and make utilization of the boards or cut pieces very easy where rigid products are unsuitable. Superwool ® HT Unifelt ™ boards are supplied in a wide range of thickness combining light weight, high heat resistance, low thermal conductivity with high sound absorption properties.

Typical applications:

  • Sealing
  • Ingot insulation
  • Expansion gaskets
  • Back-up insulation

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density <= 0.190 g/cc<= 0.00686 lb/in³
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.100 W/m-K
@Temperature 400 °C
0.694 BTU-in/hr-ft²-°F
@Temperature 752 °F
ASTM C-201
 0.150 W/m-K
@Temperature 600 °C
1.04 BTU-in/hr-ft²-°F
@Temperature 1110 °F
ASTM C-201
 0.210 W/m-K
@Temperature 800 °C
1.46 BTU-in/hr-ft²-°F
@Temperature 1470 °F
ASTM C-201
 0.300 W/m-K
@Temperature 1000 °C
2.08 BTU-in/hr-ft²-°F
@Temperature 1830 °F
ASTM C-201
Shrinkage <= 1.0 %
@Temperature 1100 °C,
Time 86400 sec
<= 1.0 %
@Temperature 2010 °F,
Time 24.0 hour
isothermal; EN-1094-1
 
Descriptive Properties
Classification Temperature (°C)1250
Colorwhite/tan

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMORF7029 / 203328

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.