MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 4009 MS 2  Polyphthalamide (PPA) Glass Fiber 50% - Molybdenum Disulfide 2%  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 50% Glass Fiber Reinforced

Material Notes: Glass Fiber 50% - Molybdenum Disulfide 2%

Comments:

  • Glass Fiber
  • Molybdenum Disulfide

Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.

Information provided by RTP Company.


Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.66 g/ccASTM D792
Filler Content 50 %
Water Absorption 0.20 %24 hours at 23°C; ASTM D570
Linear Mold Shrinkage 0.0010 cm/cm
@Thickness 3.17 mm
ASTM D955
 0.0010 cm/cm
@Thickness 6.35 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 126ASTM D785
Tensile Strength, Ultimate 33000 psiASTM D638
Elongation at Break 1.6 %ASTM D638
Modulus of Elasticity 3200 ksiASTM D638
Flexural Yield Strength 46000 psiASTM D790
Flexural Modulus 2400 ksiASTM D790
Izod Impact, Notched 1.50 ft-lb/in
@Thickness 3.17 mm
ASTM D256
Izod Impact, Unnotched 10.0 ft-lb/in
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 10.0 µin/in-°F
@Temperature 20.0 °C
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 540 °FASTM D648
Flammability, UL94 HB
@Thickness 1.59 mm
Per testing by RTP Company; ASTM D635
 
Processing PropertiesOriginal ValueComments
Processing Temperature 565 - 615 °F
Mold Temperature 275 - 325 °F
Injection Pressure 10000 - 18000 psi
 
Descriptive Properties
ColorNatural/Black

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PlastiComp Complet® LGF50-PPA Polyphthalamide, 50% Long Glass Fiber Reinforced
MTI ThermoStran® PPA-50G Long Glass Fiber Compound
LATI Latigloss 57 G/50 F2 PPA, 50% Glass Fiber Reinforced
Avient Edgetek® AM-45GF/000 PPA (Polyphthalamide), 45% Glass Fiber Reinforced, Hi-Temp
DuPont Mobility and Materials Zytel® HTN 55G55LWSF BK752A Polyphthalamide (PPA)

PR5217 / 64576

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.