MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

LyondellBasell Lupolen 5461B Q471 High Density Polyethylene (HDPE), Pipe Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: Lupolen 5461 B Q 471 is a high density polyethylene (HDPE) powder with high melt viscosity for extrusion of peroxide cross linked pipes (PE-Xa). Typical application: Cross linked pipes, PE-Xa (peroxide). Applications: Drinking Water Pipe, Plumbing, Heating & Cooling

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.953 g/cc0.0344 lb/in³ISO 1183-1
Melt Flow  0.50 g/10 min
@Load 5.00 kg,
Temperature 190 °C
0.50 g/10 min
@Load 11.0 lb,
Temperature 374 °F
measured on powder; ISO 1133-1
 10 g/10 min
@Load 21.6 kg,
Temperature 190 °C
10 g/10 min
@Load 47.6 lb,
Temperature 374 °F
measured on powder; ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 64
@Time 3.00 sec
64
@Time 0.000833 hour
ISO 868
Ball Indentation Hardness 49.0 MPa7110 psiISO 2039-1
Tensile Strength, Yield 28.0 MPa4060 psi50mm/min; ISO 527-1,-2
Elongation at Yield 8.0 %8.0 %50mm/min; ISO 527-1,-2
Tensile Modulus 1.10 GPa160 ksiISO 527-1,-2
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 79.0 °C174 °FB50; ISO 306
 130 °C266 °FA50N; ISO 306
 
Descriptive Properties
Ball Indentation Hardness (MPa)H 132/30
Processing MethodPipe, Sheet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips HiD® 9300 HDPE Orange Pipe Resin
Chevron Phillips Marlex® HP076 High Density Polyethylene, Pipe Grade
LyondellBasell Alathon L 4930TC High Denisty Polyethylene
LyondellBasell Lupolen 5031L Q449 K High Density Polyethylene (HDPE), Pipe Grade
LyondellBasell Lupolen 5461B Q471 B High Density Polyethylene (HDPE), Pipe Grade

PEQT8579 / 220214

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.