MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Celanese Nilit FRIANYL B63 FK 2010 Nylon 6 for injection molding, 20% glass fiber and 10% glass ball reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Nylon 6 for injection molding.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.33 g/ccISO 1183
Water Absorption 1.5 - 2.4 %ISO 62
Water Absorption at Saturation 6.0 - 7.0 %ISO 62
Viscosity Measurement 145Viscosity index; ISO 307
Linear Mold Shrinkage 0.0060 - 0.014 cm/cmFRISETTA Test Method
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 127 MPaISO 527
Elongation at Break 3.0 %ISO 527
Tensile Modulus 8.40 GPaISO 527
Flexural Modulus 5.90 GPaISO 178
Charpy Impact Unnotched 3.70 J/cm²DIN 53453
 2.80 J/cm²
@Temperature -40.0 °C
DIN 53453
Charpy Impact, Notched 0.800 J/cm²DIN 53453
 0.500 J/cm²
@Temperature -40.0 °C
DIN 53453
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 93
Dissipation Factor 0.020
@Frequency 1e+6 Hz
IEC 250
Comparative Tracking Index 575 VCTI 100; IEC 112
 
Thermal PropertiesOriginal ValueComments
Melting Point 221 °CISO 3146 DSC
Maximum Service Temperature, Air 110 °CContinuous; FRISETTA Test Method
Deflection Temperature at 0.46 MPa (66 psi) 220 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 210 °CISO 75

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Azoty Tarnow™ Tarnamid® T-27 GF15 MW25 Polyamide 6 - Mineral Reinforced
BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Dry)
Domo Technyl® C 218 MT25 V15 25% Mineral, 15% Glass Filled, Heat Stabilized Nylon 6
BASF Ultramid® BG40GM45 HS BK 00130 20/25 % Glass/Mineral Filled PA6 (Dry)
Envalior Akulon® K224-LGM35 PA6-(GF+MD)40, Dry, 15/25% Glass/Mineral Filled

PFRI111 / 39032

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.