MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Coat 15D UV Curable Coating Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: The TRA-COAT 15D is a clear, liquid material that cures in thick sections to a "lens-like" appearance when exposed to ultra violet light. It`s rigidity makes it an ideal material for the coating of nameplates and automotive parts. TRA-COAT 15D is a clear, non-yellowing formulation that offers low shrinkage during cure and excellent durability thereafter. With a 200 Watt/inch medium pressure mercury vapor lamp, the TRA-COAT 15D will cure at a rate of 5-10 feet per minute. Applications in which the TRA-COAT 15D has been successfully used in range from lamination of nameplates and labels, coating of plastic and metal parts for the automotive industry, lamination of circuit boards, and bonding of various optical components.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 3200 cP
@Temperature 25.0 °C
Mixed, ssa# 14, 100 rpm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75
Adhesive Bond Strength 709 psiLap shear, glass to glass
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 31.0 °CUltimate Tg
 
Descriptive Properties
Color Clear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTRAC002 / 70930

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.