MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Novablend™ 5035 Polyvinyl Chloride, Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes:

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.35 g/cc1.35 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 48.3 MPa7010 psiType I, 5.1 mm/min; ASTM D638
Tensile Modulus 3.24 GPa470 ksiType I, 5.1 mm/min; ASTM D638
Flexural Strength 86.9 MPa12600 psiASTM D790
Flexural Modulus 2.76 GPa400 ksiASTM D790
Izod Impact, Notched 0.350 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
0.656 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 67.2 °C
@Thickness 1.57 mm
153 °F
@Thickness 0.0618 in
Annealed; ASTM D648
Flammability, UL94 V-0V-0Cell classification 12453(D-1784); UL 94
Oxygen Index 30 %30 %ISO 4589-2
 
Compliance PropertiesMetricEnglishComments
FDA YesYesFood Contact, Unspecified Rating
 
Descriptive Properties
AppearanceClear/Transparent
FeaturesFood Contact Acceptable
 High Gloss
FormsPellets
Generic MaterialPVC, Rigid
Generic NamePolyvinyl Chloride, Rigid (PVC, Rigid)
Processing MethodExtrusion
Regional AvailabilityNorth America
UsesProfiles
 Transparent or Translucent Parts

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Axiall Tuf-Stif 2802 Rigid PVC, Extrusion
Axiall 2512 Rigid PVC, Extrusion
Axiall 5006 Rigid PVC, Extrusion, Natural
Avient Novablend™ 9562 Polyvinyl Chloride Alloy (PVC Alloy)
Avient Novablend™ 6602 Polyvinyl Chloride, Rigid

PH0POL1089 / 145658

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.