MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Danquinsa DANMELTTHANE® PES-700 Adhesive
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: DANMELTTHANE_ PES-700 is a linear, saturated, high molecular, solvent free polyester. This partly crystalline polyester type is applied as a basic raw material by the production of reactive hot melt adhesives, for lamination adhesives and for the lamination of foils. DANMELTTHANE_ PES-700 is also suitable for the processing of thermoplastic PUR- granules and lacquers.

Application: DANMELTTHANE_ PES-700 is used by the processing of reactive polyurethane- hot melt adhesives. A further application field is the production of hot melt adhesives or solvent containing adhesives needed by the laminations of foils. DANMELTTHANE_ PES-700 molten and/or dissolved is applied for the lamination of textiles or as an equipment for adhesives. For the lamination of textiles and the equipment of adhesives we recommend the application by hot spray lamination. Further produced are release lacquer coatings, high elastic CC-Primer and rotograve gravure lacquer.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³DIN 53.479
Brookfield Viscosity 15000 cP
@Temperature 230 °C
15000 cP
@Temperature 446 °F
RVT
Molecular Weight 25000 - 27000 g/mol25000 - 27000 g/molDIN 53735
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 2.0<= 2.0[mg KOH/g]
 
Thermal PropertiesMetricEnglishComments
Melting Point 85.0 - 90.0 °C185 - 194 °FKOFLER
Glass Transition Temp, Tg -19.0 - -15.0 °C-2.20 - 5.00 °FDSC
 -4.00 °C24.8 °FDSC-Cooling
 5.50 °C41.9 °FDSC-Heating
Flash Point 230 °C446 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
Aspecttransparent to slightly yellow solid material
Color3DIN 6162
OH-number2 mg KOH/g
Thickening point40°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDANQ127 / 294547

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.