MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® HexWeb® HRH-327 - 1/8 - 3.2 Fiberglass Reinforced Polyimide Honeycomb
Categories: Other Engineering Material; Composite Fibers; Polymer; Thermoset; Polyimide, TS

Material Notes: Designation: Material-Cell Size (inches)-Density
HexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well as both the initial and final web impregnations. This material has been developed for extended service temperatures up to 500°F with short-term capabilities up to 700°F. Unless other specified, material will have standard postcure.

Features: High-strength retention up to 500°F continuous service; 700°F short and intermittent term exposures; All polyimide resin and adhesive system; Good dielectric properties; Good insulative properties; Compatible with Hexcel polyimide adhesive, foam, and prepreg.
Applications: A high-temperature nonmetallic honeycomb for use in sandwich structures that require good electrical properties or that see service temperatures in the range of 350°F-500°F. Applications include sandwich structures for Mach 2 and Mach 3 aircraft, high-energy radomes, structural and acoustical engine inlets and liners.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.20 lb/ft³
 
Mechanical PropertiesOriginal ValueComments
Compressive Yield Strength >= 0.220 ksiStabilized, min
 0.310 ksiStabilized, typical
Compressive Modulus 27.0 ksiStabilized, typical
Shear Modulus 7.50 ksiPlate Shear, W Direction, typical
 19.0 ksiPlate Shear, L Direction, typical
Shear Strength >= 0.0700 ksiPlate Shear, W Direction, min
 0.0950 ksiPlate Shear, W Direction, typical
 >= 0.140 ksiPlate Shear, L Direction, min
 0.195 ksiPlate Shear, L Direction, typical
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 500 °FExtended
 700 °FShort Term

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mid-Mountain Materials HYTEX® 5000 High Carbon Industrial Textile (PAN)
Fiberglass Search Hints
PCC-Advanced Forming Technology 63% AlSiC Metal Matrix Composite
Poly-u-Mac GatorBoard WR-26 Fiberglass Reinforced Foam
Hexcel® HexForce™ 3783 Fiber Glass Fabric

PHEXC389 / 98860

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.