MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Syensqo (Solvay Specialty Polymers) Fomblin® DA305 Perfluoropolyether
Categories: Fluid; Lubricant; Perfluoropolyether (PFPE)

Material Notes: Fomblin® DA305 is the optimum product for use with greases. Solutions of Fomblin® PFPE lubricants formulated with 5% (wt.) of DA305 are clear and stable in storage for over 1 year. These blends can be used in exactly the same manner as non-additivated Fomblin® lubricants for the production of greases. The physical properties of greases additivated with DA305 remain practically unchanged compared to those of the non-additivated greases; volatility may increase slightly, depending on the base fluid, and oil separation may decrease.
Depending on the base fluid, these greases can be used at temperatures ranging from -70 to 250 °C.

Features: Chemical Resistant; High Density; High Heat Resistance

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Molecular Weight 3800 g/mol3800 g/molAverage
Vapor Pressure 3.33e-7 bar
@Temperature 100 °C
0.000250 torr
@Temperature 212 °F
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature 270 - 300 °C518 - 572 °FThermal Stability
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
FormsLiquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4181 / 279981

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.