MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PTS PBT-1100A PBT Resin
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant

Material Notes:

Information provided by PTS LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.29 - 1.33 g/cc1.29 - 1.33 g/ccISO 1183
Moisture Absorption at Equilibrium <= 0.3 %<= 0.3 %ISO 15512
Viscosity Test 1.03 - 1.07 cm³/g0.0103 - 0.0107 dl/gISO 1628/5
Ash <= 0.035 %<= 0.035 %ISO 3451/1
 
Thermal PropertiesMetricEnglishComments
Melting Point 222 - 226 °C432 - 439 °FISO 11357
 222 - 226 °C432 - 439 °FISO 11357
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.30 %<= 0.30 %ISO 15512
 
Descriptive Properties
Carboxyl End Groups< 30 mol/tQ/NHS 501
Color B< 6.0Hunter Lab

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PTS PCA-3015 Low Temperature Impact PC/PBT Alloy
PTS PCA-3013 High Flow PC/PBT Alloy
PTS PBT-30GF 30% Glass Fiber Reinforced PBT
A. Schulman ComAlloy Hiloy® 415 Polyester - PBT, Glass Reinforced
A. Schulman VOLOY™ 462 Hybrid Reinforced PBT Alloy

PZ9PU909 / 135367

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.