MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Akro-Plastic Akromid® A3 S1 black 950089 (1071) Unreinforced Nylon 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes: Unreinforced. High toughness. PA 6.6-I.

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.013 - 0.015 cm/cm0.013 - 0.015 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.015 - 0.017 cm/cm0.015 - 0.017 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 40.0 MPa5800 psi50 mm/min; Conditioned; ISO 527-2
 50.0 MPa7250 psi50 mm/min; Dry as Molded; ISO 527-2
Elongation at Break >= 50 %>= 50 %50 mm/min; Dry as Molded; ISO 527-2
 >= 100 %>= 100 %50 mm/min; Conditioned; ISO 527-2
Tensile Modulus 0.900 GPa131 ksi1 mm/min. Conditioned; ISO 527-2
 2.00 GPa290 ksi1 mm/min. Dry as Molded.; ISO 527-2
Flexural Modulus 1.95 GPa283 ksi2 mm/min. Dry as Molded; ISO 178
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Dry as molded; ISO 179-1/1eA
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Conditioned; ISO 179-1/1eA
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Dry as molded; ISO 179-1/1eA
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Conditioned; ISO 179-1/1eA
Charpy Impact, Notched  >= 3.50 J/cm²
@Temperature -30.0 °C
>= 16.7 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179-1/1eA
 >= 3.50 J/cm²
@Temperature -30.0 °C
>= 16.7 ft-lb/in²
@Temperature -22.0 °F
Dry as Molded; ISO 179-1/1eA
 >= 8.00 J/cm²
@Temperature 23.0 °C
>= 38.1 ft-lb/in²
@Temperature 73.4 °F
Dry as Molded; ISO 179-1/1eA
 >= 10.0 J/cm²
@Temperature 23.0 °C
>= 47.6 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179-1/1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.00e+14 ohm1.00e+14 ohmDry as Molded; IEC 60093
 
Thermal PropertiesMetricEnglishComments
Melting Point 262 °C504 °FDry as Molded. DES, 10°C/min; DIN EN 11357-1
Deflection Temperature at 0.46 MPa (66 psi) 152 °C306 °FDry as Molded; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C158 °FDry as Molded; ISO 75
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Conditioned
 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Dry as Molded
 
Descriptive Properties
Burning Rate<100 mm/minDry as Molded. FMVSS 302. >1 mm thickness
 <100 mm/minConditioned. FMVSS 302. >1 mm thickness

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKRO9804 / 255461

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.