Features: Improved impact strength in polypropylene; Excellent filler acceptance; Available as pellet form; Outstanding toughness with flexible performance; and Reduction of product weight Application: General purpose thermoplastic elastomers, Polymer modification CSA No. 25087-34-7 Information provided by LG Chemical |