Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: Low Gloss Uses:Automotive Interior Parts Automotive Specifications: GM TMP.VM.004AA Form: Pellets Processing Method:Extrusion Information provided by Teknor Apex |