MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil SpectraSyn™ 8 Polyalphaolefin (PAO) Fluid
Categories: Fluid; Lubricant; Polyalphaolefin (PAO)

Material Notes: Product Description: SpectraSyn™ Low Viscosity Polyalphaolefin (PAO) basestocks feature low temperature properties, low volatility, and improved thermal stability. SpectraSyn™ Low Viscosity (PAO) products have high viscosity indices which translate to improved flow at low temperatures and increased film thickness at high temperatures. SpectraSyn™ Low Viscosity PAO products are the primary basestocks for synthetic lubricants used in passenger car engines, heavy-duty diesel engines, transmissions, gear boxes and a variety of industrial applications.

Appearance: Bright & Clear

Availability: Africa & Middle East, Asia Pacific, Central America, Europe, North America and South America

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.833 g/cc
@Temperature 15.6 °C
0.0301 lb/in³
@Temperature 60.1 °F
ASTM D4052
Viscosity <= 2.58 cP<= 2.58 cPHigh-Temp. High Shear; ASTM D5481
 <= 16200 cP
@Temperature -40.0 °C
<= 16200 cP
@Temperature -40.0 °F
Apparent Viscosity by Mini-Rotary Viscometer; ASTM D4684
Brookfield Viscosity 17590 cP
@Temperature -40.0 °C
17590 cP
@Temperature -40.0 °F
ASTM D2983
Viscosity Measurement 139139Index; ASTM D2270
Kinematic Viscosity 19000 cSt
@Temperature -40.0 °C
19000 cSt
@Temperature -40.0 °F
ASTM D445
Kinematic Viscosity at 40°C (104°F) 48 cSt48 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 8.0 cSt8.0 cStASTM D445
Vapor Pressure 0.000133 bar
@Temperature 150 °C
0.100 torr
@Temperature 302 °F
ASTM D2879
Evaporation Loss  0.80 %
@Temperature 150 °C,
Time 79200 sec
0.80 %
@Temperature 302 °F,
Time 22.0 hour
ASTM D972
 5.5 %
@Temperature 205 °C,
Time 23400 sec
5.5 %
@Temperature 401 °F,
Time 6.50 hour
ASTM D972
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.050<= 0.050[mg KOH/g]; ASTM D974 (mod)
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.122.12ASTM D924
Dielectric Breakdown 37700 V37700 V
 
Thermal PropertiesMetricEnglishComments
Pour Point -47.8 °C-54.0 °FASTM D5950/D97
Flash Point 260 °C500 °FCOC; ASTM D92
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.46051.4605ASTM D1218
 
Descriptive Properties
Aniline Point267.4°FASTM D611
Cold Cranking Simulator4800 cP-22°F, ASTM D5293
Color<0.5ASTM D1500
CompositionWater<50 ppm, ASTM D6304 (mod)
Density Correction Factor0.000624 (g/cc)/°CASTM D1250
Fire Point547°FCOC, ASTM D92
Noack Volatility (%)4.1ASTM D5800/DIN 51581

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil SpectraSyn™ 4 Polyalphaolefin (PAO) Fluid
ExxonMobil SpectraSyn Plus™ 6 Advanced Polyalphaolefin (PAO) Fluid
ExxonMobil SpectraSyn Plus™ 4 Advanced Polyalphaolefin (PAO) Fluid

PEX99695 / 175931

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.