MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M 9039 Double Coated Tapes with Adhesive 300
Categories: Polymer; Adhesive

Material Notes: 3M™ Double Coated Tapes with 3M™ Adhesive 300 feature a thin polyester film for dimensional stability and improved handling with ease of die cutting and laminating. The high tack adhesive provides relatively high initial adhesion and good shear holding power to a variety of surfaces. The carrier also provides easier handling during slitting and die cutting.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 12.7 microns0.500 milCarrier
 38.1 microns1.50 milFaceside Adhesive
 38.1 microns1.50 milBackside Adhesive
 76.2 microns3.00 milLiner Caliper
 88.9 microns3.50 milTape
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.73407 kN/m4.1875 plito stainless steel, 90°, 15 min RT; ASTM D3330
 0.79981 kN/m4.5625 plito ABS, 90°, 2 mil al foil, 72 hr RT; ASTM D3330
 0.84363 kN/m4.8125 plito Polyester, 90°, 2 mil al foil, 72 hr RT; ASTM D3330
 0.877 kN/m5.00 plito Polycarbonate, 90°, 2 mil al foil, 72 hr RT; ASTM D3330
 0.8984 kN/m5.125 plito stainless steel, 90°, 72 hr RT; ASTM D3330
 1.074 kN/m6.125 plito stainless steel, 90°, 72 hr at 70°C; ASTM D3330
 1.4134 kN/m8.0625 plito stainless steel, 180°, 2 mil al foil, 72 hr RT; ASTM D3330
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 82.0 °C180 °FLong term
 121 °C250 °FShort term
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM33270 / 168017

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.