MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Kaowool™ Blanket S
Categories: Ceramic; Oxide

Material Notes: Kaowool™ Blanket S and SZr are made from bulk fibers produced by the most modern spinning process. This produces fibers of exceptional length and uniform distribution which are ideal for manufacturing blanket of controlled density, high tensile strength and resiliency.

Applications:

  • Furnace linings - all industries: iron & steel, non-ferrous, aluminium, bricks and ceramics/pottery
  • Petrochemical: crackers, heaters and ducts
  • Cladding/lining waste-heat ducts
  • Cladding of exhausts
  • Acoustic insulation
  • Steam turbine insulation
  • Hot boxes
  • Domestic appliances
  • Automobiles/vehicles

Information provided by Morgan Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.640 - 1.60 g/cc
@Temperature 23.0 °C
50% RH; EN 1094-1
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 3.82 MPaat 64kg/m3; NF-B-40-456
 7.65 MPaat 96kg/m3; NF-B-40-456
 10.1 MPaat 128kg/m3; NF-B-40-456
 12.45 MPaat 160kg/m3; NF-B-40-456
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0600 W/m-K
@Temperature 200 °C
at 128kg/m3
 0.0600 W/m-K
@Temperature 200 °C
at 96kg/m3
 0.0700 W/m-K
@Temperature 200 °C
at 64kg/m3
 0.100 W/m-K
@Temperature 400 °C
at 128kg/m3
 0.110 W/m-K
@Temperature 400 °C
at 96kg/m3
 0.120 W/m-K
@Temperature 400 °C
at 64kg/m3
 0.150 W/m-K
@Temperature 600 °C
at 128kg/m3
 0.160 W/m-K
@Temperature 600 °C
at 96kg/m3
 0.200 W/m-K
@Temperature 800 °C
at 128kg/m3
 0.200 W/m-K
@Temperature 600 °C
at 64kg/m3
 0.230 W/m-K
@Temperature 800 °C
at 96kg/m3
 0.270 W/m-K
@Temperature 1000 °C
at 128kg/m3
 0.300 W/m-K
@Temperature 800 °C
at 64kg/m3
 0.320 W/m-K
@Temperature 1000 °C
at 96kg/m3
 0.430 W/m-K
@Temperature 1000 °C
at 64kg/m3
Shrinkage 1.5 %
@Temperature 1000 °C,
Time 86400 sec
NF-B-40-452
 2.2 %
@Temperature 1100 °C,
Time 86400 sec
NF-B-40-452
 3.0 %
@Temperature 1200 °C,
Time 86400 sec
NF-B-40-452
 5.5 %
@Temperature 1300 °C,
Time 86400 sec
NF-B-40-452
 
Component Elements PropertiesOriginal ValueComments
Al2O3 44 %
CaO+MgO 0.050 %
K2O+Na2O 0.10 %
Other 0.15 %Fe2O3 + TiO2
SiO2 56 %
 
Descriptive Properties
Classification Temperature (°C)1260
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NuSil MED3-4800 Master Batches - Unrestricted Medical Use
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
DAK Americas Laser+® C91A PET
Thermal Ceramics Kaowool Blanket, Blanket S Mesh Enclosed Rounds, Strips and Blankets
Wellman ThermaClear® Ti818 (0.79 IV) PET

CMORF7049 / 203348

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.