Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America Additive: Impact Modifier; Plasticizer Features: Good Flexibility; High Impact Resistance; High Viscosity; Impact Modifier; Light Stabilized; UV Resistant Uses: Automotive Applications; Hydraulic Applications Appearance: Natural Color Forms: Granules Processing Method: Extrusion; Profile Extrusion Information provided by EMS-Grivory |