MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
North American White Fir Wood
Categories: Wood and Natural Products; Wood; Softwood

Material Notes: Data is based on small, clear, air-dried samples unless specified.

Property values marked by an asterisk (*) have been taken from an unusually old reference source.

Key Words: Abies concolor; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.350 g/ccOven Dry Weight/Unseasoned Volume
 47.0 lb/ft³Unseasoned*
 
Mechanical PropertiesOriginal ValueComments
Hardness, Wood Indentation 1500 NSide. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 1700 NEnd. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 2100 NSide
Tensile Strength, Ultimate 1.80 MPaPerpendicular to Grain
 260 psiPerpendicular to Grain*
Modulus of Rupture 0.0640 GPaStatic Bending
 6.00 ksiStatic Bending*
Flexural Yield Strength 3900 psiFiber Stress at Elastic Limit; Static Bending*
Flexural Modulus 9.52 GPaStatic Bending
 1130 ksiStatic Bending*
Compressive Strength 4.10 MPaPerpendicular to Grain
 37.0 MPaParallel to Grain
 440 psiPerpendicular to Grain*
 2610 psiParallel to Grain*
 2800 psiMax Crushing Strength Parallel to Grain*
Shear Strength 6.40 MPaOrientation Unknown
 730 psiParallel to Grain*
Impact 2.2in-lb/in³; Work to Elastic Limit; Unseasoned Sample; Impact Bending*
 7200psi; Fiber Stress at Elastic Limit; Unseasoned Sample; Impact Bending*
Work to Elastic Limit 0.770 in-lb/in³Static Bending*
Work to Maximum Load 5.20 in-lb/in³Static Bending*
Toughness 14.7 JRadial
 22.6 JTangential
Cleavage 25.0 kN/mRadial surface of failure, Unseasoned*
 33.0 kN/mTangential surface of failure, Unseasoned*
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.680 BTU-in/hr-ft²-°FOven Dry
 0.820 BTU-in/hr-ft²-°F12% Moisture Content
Shrinkage 3.2 %Radial; Green to Zero Moisture
 7.1 %Tangential; Green to Zero Moisture
 9.8 %Volumetric; Green to Zero Moisture

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
European White Fir Wood
Interior North Douglas Fir Wood
European Grecian Fir Wood
Northern White Pine Wood
American Rocky Mountain Douglas Fir Wood

PTSA630 / 71269

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.