MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
INEOS Styrolution Luran® VLN SAN
Categories: Polymer; Thermoplastic; SAN Polymer; Styrene Acrylonitrile (SAN), Transparent

Material Notes: Description: Luran® VLN is a styrene/acrylonitrile copolymer without any lubricants particularly suitable for ABS compounds. Luran® VLN is an easy flowing SAN grade especially suited for injection molding ABS compounds. Due to its low acrylonitrile content, ABS compounds with good compatibility to polycarbonate are accessible.

Information provided by STYROLUTION, which is a joint venture between BASF and INEOS

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccASTM D 792
Melt Flow 70 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 122ASTM D 785
Tensile Strength, Yield 69.0 MPaASTM 638
Elongation at Break 3.0 %Failure; ASTM 638
Flexural Strength 100 MPaASTM D 790
Flexural Modulus 3585 MPaASTM D 790
Izod Impact, Notched 0.340 ft-lb/in
@Temperature 23.0 °C
ASTM D 256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 97.0 °CUnannealed; ASTM D648
 100 °CAnnealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 89.0 °CUnannealed; ASTM D648
 97.0 °CAnnealed; ASTM D648
Vicat Softening Point 100 °C
@Load 1.02 kg
VST/A/50. 50C/h; ISO 306
 
Descriptive Properties
ColorNatural

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema OREVAC® 18910 Maleic Anhydride Modified Copolymer
Aclo Accutech SAN SAN930G10L Glass Reinforced
Aclo Accucomp SAN SAN900L
Dow Tyril® 100 SAN
INEOS Styrolution Luran® S KR2866C ASA / PC

PBASG0601 / 132234

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.