MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 3400 FC-120 Liquid Crystal Polymer (LCP) Glass Fiber - Mineral  (discontinued **)
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP)

Material Notes: Information provided by RTP Company.


Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Water Absorption 0.10 %24 hrs @ 23°C; ASTM D 570
Linear Mold Shrinkage 0.0020 cm/cm
@Thickness 3.17 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 15000 psiASTM D 638
Elongation at Break 1.4 %ASTM D 638
Tensile Modulus 2.50e+6 psiASTM D 638
Flexural Strength 20000 psiASTM D 790
Flexural Modulus 2.50e+6 psiASTM D 790
Izod Impact, Notched 1.20 ft-lb/in
@Thickness 3.17 mm
ASTM D256
Izod Impact, Unnotched 6.00 ft-lb/in
@Thickness 3.17 mm
ASTM D4812
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 600 °FASTM D 648
Flammability, UL94 V-0
@Thickness 1.59 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 685 - 750 °F
Mold Temperature 150 - 250 °F
Drying Temperature 300 °F8 hrs
Dew Point -20.0 °F
Injection Pressure 15000 - 20000 psi

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LNP Lexan® SML5861 Polycarbonate, 14% Glass / Mineral Reinforced
Lavergne VYPET VNT 245 PET - PBT 45% Glass Reinforced Polyester
Celanese Zenite® 6635 BK010 LCP
Celanese Zenite® 6330 NC010 LCP (Extended Tabular Temperature Data)
Celanese Vectra® A410 Liquid Crystal Polymer (LCP), 25% Glass/25% Mineral Filled

PQZZ2517 / 61022

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.