System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
LG Chemical LUCON PA6110EM PC+CNT+GF, Injection Molding
Categories:
Polymer
;
Thermoplastic
;
Polycarbonate (PC)
;
Polycarbonate, 10% Glass Filled
Material Notes:
Electromagnetic Interference (EMI) Shielding, EMI absorption,
Application: Radar housing, Blind Spot Detection (BSD) shielding for automotive
Information provided by LG Chemical
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.25
-
1.35
g/cc
0.0452
-
0.0488
lb/in³
ASTM D792
Linear Mold Shrinkage, Flow
0.0030
-
0.0050
cm/cm
@Thickness 3.20 mm
0.0030
-
0.0050
in/in
@Thickness 0.126 in
ASTM D955
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
125
MPa
@Thickness 3.20 mm
18100
psi
@Thickness 0.126 in
5mm/min; ASTM D638
Elongation at Break
<= 3.0 %
@Thickness 3.20 mm
<= 3.0 %
@Thickness 0.126 in
5mm/min; ASTM D638
Flexural Strength
190
MPa
@Thickness 6.40 mm
27600
psi
@Thickness 0.252 in
3mm/min; ASTM D790
Flexural Modulus
4.80
GPa
@Thickness 6.40 mm
696
ksi
@Thickness 0.252 in
3mm/min; ASTM D790
Izod Impact, Notched
0.450
J/cm
@Thickness 6.40 mm
0.843
ft-lb/in
@Thickness 0.252 in
ASTM D256
Electrical Properties
Metric
English
Comments
Surface Resistance
1.00e+7
-
1.00e+11
ohm
1.00e+7
-
1.00e+11
ohm
IEC 60093
Shielding Effectiveness
3.0
-
6.0
dB
@Thickness 3.00 mm
3.0
-
6.0
dB
@Thickness 0.118 in
ASTM D4935
Thermal Properties
Metric
English
Comments
Deflection Temperature at 1.8 MPa (264 psi)
203
°C
@Thickness 6.40 mm
397
°F
@Thickness 0.252 in
Unannealed; ASTM D648
Processing Properties
Metric
English
Comments
Rear Barrel Temperature
230
-
250
°C
446
-
482
°F
Middle Barrel Temperature
240
-
270
°C
464
-
518
°F
Front Barrel Temperature
240
-
270
°C
464
-
518
°F
Nozzle Temperature
250
-
280
°C
482
-
536
°F
Melt Temperature
250
-
280
°C
482
-
536
°F
Mold Temperature
80.0
-
100
°C
176
-
212
°F
Drying Temperature
80.0
-
100
°C
@Time 14400 - 18000 sec
176
-
212
°F
@Time 4.00 - 5.00 hour
Back Pressure
0.000
-
0.981
MPa
0.000
-
142
psi
Screw Speed
40
-
80
rpm
40
-
80
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PLHCHEM9821 / 239337
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.